Fabrication

Solution Annealed Room Temperature Hardness

Form Hardness Typical ASTM Grain Size
Sheet 93 HRBW 5 - 6.5
Plate 29 HRC 5.5 - 6.5

All samples tested in solution-annealed condition
HRBW = Hardness Rockwell “B”, Tungsten Indentor.
HRC = Hardness Rockwell “C”.

Waspaloy, Solution Annealed, Room Temperature Tensile

Form Test Temperature 0.2% Yield Strength Ultimate Tensile Strength 4D Elongation
°F °C ksi MPa ksi MPa %
Sheet RT RT 60.8 419 131.9 909 52.2
Plate RT RT 87.6 604 154.7 1067 42.3